Special element ratio of bimetallic hammer head

2026-04-12 222

The special element ratio of bimetallic hammer heads is mainly reflected in optimizing material properties through multi-element alloys, as follows:

Core wear-resistant element combination

The working part of the hammer head (high chromium cast iron) usually contains elements such as chromium (19.3-26%), molybdenum (1.96%), vanadium (0.01-0.6%), copper (0.98%), etc. Chromium improves hardness and wear resistance, molybdenum enhances high-temperature stability, vanadium refines grain size, and copper improves corrosion resistance.

Rare earth and trace alloy elements

Adding trace alloys such as rare earths, titanium, antimony, niobium, and tungsten to further refine grain size and purify metal structure, enhancing wear resistance and impact resistance. For example, rare earth elements can optimize grain boundary structure and reduce brittleness.

Proportion of tough material for hammer handle

The hammer handle (made of low-alloy steel) contains carbon (0.35-0.45%), manganese (0.8-1.2%), molybdenum (0.4-0.8%), and chromium (4.0-6.0%), balancing toughness and strength to ensure impact resistance without fracture.

Elements related to heat treatment process

By optimizing the heat treatment effect with elements such as nickel (0.5-1.0%), vanadium (0.3-0.6%), and nitrogen (0.05-0.1%), the hardness can reach HRC62-65 while maintaining toughness.

Interface strengthening of composite technology

The liquid-liquid composite casting technology ensures a metallurgical fusion rate of over 99% at the interface between the two alloys, avoiding the risk of fracture.