The main reason for the hardness of the hammer head not meeting the standard

1、 Abnormal composition of raw materials
Insufficient chromium content: The chromium (Cr) content in the working end of high chromium alloys is less than 15% (ideal range is 15% -26%), resulting in the inability to form sufficient high hardness carbides (such as Cr ₇ C ∝), which directly affects the hardening ability. Some counterfeit products are disguised as low chromium cast iron or high manganese steel, with a hardness generally lower than HRC 50.
Excessive impurity elements: sulfur (S), phosphorus (P) and other elements segregate to form brittle phases, which damage the continuity of the matrix, reduce local hardness and cause microcracks.
Carbon content imbalance: When the carbon content is below 0.6%, there is insufficient precipitation of carbides; Above 0.8%, coarse carbides are prone to occur, leading to increased brittleness and uneven hardness distribution.
2、 Defects in casting process
Poor bonding at the composite interface: During the dual liquid casting process, the temperature difference between the high chromium alloy liquid and the low carbon steel liquid is too large or the time is delayed, resulting in the interface not achieving metallurgical bonding, forming oxide interlayers or pores, and weakening the overall hardness transfer.
Uncontrolled casting temperature: The pouring temperature of high chromium alloy liquid is below 1450 ° C, resulting in poor fluidity and easy occurrence of shrinkage porosity and cold insulation; If the temperature is too high, it will intensify oxidation and decarburization, forming a surface softening layer.
Uneven cooling rate: Poor thermal conductivity or insufficient cooling time of the mold can lead to coarse structure, incomplete martensitic transformation, increased residual austenite, and decreased hardness.
3、 Error in heat treatment process
|Heat treatment process | Failure behavior | Hardness influence mechanism|
| --- | --- | --- |
|Insufficient quenching temperature | Not reaching the critical point of Ac ₁ (about 800-850 ° C) | Insufficient martensitic transformation, residual ferrite or pearlite in the structure, hardness lower than HRC 55|
|The insulation time is too short | The carbides are not fully dissolved | The carbon concentration in the matrix is insufficient, and the hardness after quenching does not meet the standard|
|Slow cooling rate | Use air cooling instead of oil quenching | Transform products into pearlite or bainite, with significantly lower hardness than martensite|
|Tempering temperature too high | Tempering temperature exceeding 200 ° C | Martensitic decomposition, carbide aggregation and growth, hardness decrease of 3-8 HRC|
4、 Microstructural defects
Abnormal precipitation of carbides:
Coarse M ₇ C Ⅲ carbides (>500 μ m): distributed in a continuous network, becoming a crack source, reducing overall toughness and effective hardness.
Secondary carbide deficiency: Without destruction treatment (1000 ° C insulation), dispersed precipitates such as M ₂ ∝ C ₆ did not form, and the matrix reinforcement was insufficient.
Pores and cracks:
Casting pores and shrinkage cavities as stress concentration points can induce microcracks under impact loads, resulting in abnormally low local hardness measurements.
Microcracks at the composite interface can block stress transmission, resulting in a "virtual high" hardness at the working end but a loss of actual load-bearing capacity.
5、 Detection and misjudgment factors
Measurement position error: Mismeasured hammer handle (hardness should be HRC 30-40) or transition zone, misjudged as "hardness not up to standard".
Improper detection method:
The hardness tester is not vertically compressed, or there is oil or oxide scale on the contact surface;
Failure to use standard calibration blocks for regular calibration resulted in instrument drift leading to low readings.
Insufficient representativeness of the sample: Only a single point was tested, and the average value of more than 3 points was not taken according to the requirements of GB/T 17394.1, ignoring tissue heterogeneity.
Industry Empirical Case (Local Feedback from Linyi, Shandong)
Quality Analysis of a Foundry in Linyi in 2025:
12% of the hardness non-conforming products are caused by a temperature control deviation of ± 30 ° C in the heat treatment furnace, resulting in a hardness fluctuation of ± 5 HRC in the same batch;
8% of the raw materials are mixed, and Cr12 material (with a Cr content of 12%) is mistakenly used instead of Cr26, resulting in a hardness of only HRC 52-54;
Due to the failure to apply pressure in a timely manner after pouring, a delamination of 0.1-0.3mm occurred at the composite interface, and clear boundary gaps were observed in metallographic examination.
Linyi Tiankuo Casting is a manufacturer of bimetallic hammerheads in Linyi, specializing in bimetallic hammerheads, ceramic composite hammerheads, crusher hammerheads, high chromium alloy hammerheads, wear-resistant hammerheads, alloy hammerheads, wear-resistant composite hammerheads, bimetallic composite hammerheads, composite hammerheads, bimetallic composite castings, multi-element alloy wear-resistant steel, ultra-high chromium wear-resistant castings and other products.