How to choose a suitable bimetallic hammer head?

2024-10-13 102

The selection of a suitable bimetallic hammer head should be systematically evaluated based on four dimensions: operating conditions, equipment type, material technology, and quality verification, to avoid making decisions solely based on price. The following is a structured selection guide:

image.png

1. Working condition matching: Material hardness and impact strength determine the material benchmark

High hardness materials (such as granite, basalt, iron ore, with compressive strength>200MPa)

→ Priority should be given to high chromium alloy working ends (Cr content ≥ 15%, recommended Cr18-26%), with a hardness of HRC58-65 and an increase in wear resistance by 3-5 times.

Medium hard materials (such as limestone, coal gangue, compressive strength ≤ 200MPa)

Cr12-15% high chromium alloy can be selected to balance cost and lifespan.

High frequency impact conditions (impact frequency 350-500Hz, such as sand making machines and large crushers)

The handle of the hammer must be made of high toughness alloy steel (such as 40CrMo or high manganese steel Mn13Cr2), with a hardness controlled between HRC30-40, to ensure impact resistance and prevent brittle fracture.

Low temperature/corrosive environment (such as high-altitude mines, chemical plants)

Select products that have undergone dynamic heat treatment and inorganic binder ceramic sand shell molding process (such as Linyi Tiankuo), with impact toughness ≥ 15J/cm ² at low temperatures and significantly improved corrosion resistance.

2. Equipment adaptation: Differences in selection between hammer and impact crushers

|Equipment type | Hammer head structure requirements | Process focus | Applicable scenarios|

|Hammer crusher | Suspended swinging hammer, single point impact | Hammer head working end thickness ≥ 50mm, uniform wear-resistant layer | Crushing medium hard materials, with coarse discharge particle size requirements, such as sand and gravel yards and cement plants|

|Counterattack crusher | rigid plate hammer, overall inertial impact | The hammer body needs to have high toughness as a whole to avoid fracture; Recommended forging or precision casting | crushing high hardness and brittleness materials, requiring high particle quality, such as building aggregate shaping|

✅  Key reminder: Counterattack equipment requires higher toughness of the hammer head, and the use of pure high chromium cast iron hammer heads is prohibited. It must be a bimetallic composite structure.

3. Process and Standards: Three Core Indicators that Must be Verified

Composite process:

It must be cast in one go for liquid-liquid composite, without welding or inlaying. Confirm the metallurgical bonding transition zone (continuous element gradient) through metallographic examination to eliminate the risk of interface detachment.

Hardness distribution:

Working end: HRC58-65 (measured by Rockwell hardness tester)

Hammer handle: HRC30-40 (prevents breakage)

Reject the "surface quenching virtual label" product and request multiple hardness testing reports.

Material composition:

Requesting a spectral analysis report to confirm that the content of elements such as Cr, Mn, Mo, and V meets the GB/T 24187-2009 standard (Cr ≥ 15%, impact toughness ≥ 12J/cm ²).

✅  User feedback: A sand and gravel factory in Linyi uses Tiankuo bimetallic hammer heads, which have been continuously operated for 7200 hours without replacement, reducing replacement frequency by 60% and overall operation and maintenance costs by 45%.

Selection Decision Process Diagram (Recommended Execution Order)

Confirm material hardness → 2 Identify device type → 3 Select process type (liquid-liquid composite) → 4 Verification and testing report → 5 Compare prices and supply cycles → 6 Small batch trial verification