The heat treatment process of Tiankuo bimetallic hammer head is a key link in its manufacturing process, aiming to balance the high wear resistance of the hammer head working parts (high chromium alloy) and the impact resistance of the hammer handle parts (tough material). The following are the core process points for integrating multiple sources:

1. Core steps of heat treatment
Heating and insulation
Heat the hammer head to 950-1000 ℃ (such as high chromium cast iron) and maintain it for a certain period of time (depending on the size) to uniformly austenitize the material structure and prepare for subsequent quenching.
Attention: Heating should be carried out slowly to avoid cracking caused by thermal stress (high chromium cast iron has poor thermal conductivity).
The heat treatment process of bimetallic hammer heads is part of their manufacturing process
quench cooling
Fog quenching cooling: A special fog quenching device is used for rapid cooling, forming a high hardness martensitic structure in high chromium parts, with a hardness of up to 62-65HRC.
Air cooling replacement: Some processes choose air cooling (such as lost foam casting), but the cooling rate needs to be controlled to ensure toughness.
tempering
After quenching, low-temperature tempering (200-300 ℃) is required to eliminate internal stress and improve toughness. For example:
Tempering at 250-300 ℃ (lost foam casting process);
Tempered at 200-260 ℃ (Tiankuo Hammer Head).
2. Key points of process optimization
Pearlite pretreatment: For high chromium cast iron, it can be heated to above 750 ℃ for insulation, and then slowly cooled to promote uniform precipitation of carbides and shorten the subsequent instability treatment time.
Bimetallic interface treatment: Heat treatment should ensure a strong bond between the two metals to avoid delamination caused by differences in thermal expansion coefficients.
3. Summary
The core of heat treatment for Tiankuo bimetallic hammer head is high-temperature quenching+low-temperature tempering. Through precise temperature control and cooling methods, the performance matching of "high hardness of hammer head and high toughness of hammer handle" has been achieved. The actual parameters need to be adjusted according to the material composition (such as chromium content), size, and casting process (such as lost foam/sand mold).