1、 Hammer's own factors
Material defects
If the hardness is too high, the toughness will be insufficient (such as high chromium cast iron being prone to fracture), and if the hardness is too low, the wear resistance will be poor (such as ordinary high manganese steel being prone to deformation).
Best solution: Adopt composite materials (high toughness alloy steel for hammer handle and high chromium cast iron for hammer head) or bimetallic structure, balancing hardness and toughness.

Manufacturing process issues
Casting defects (shrinkage, cracks, coarse grains) reduce the strength of the hammer head, accelerate wear and even fracture.
Improper heat treatment leads to insufficient hardening layer and decreased wear resistance.
Unreasonable structural design
When the thickness of the hammer head is too large, the hardenability is poor and the wear-resistant layer is thin; Geometric shape affects the distribution of impact force, and improper design exacerbates local wear.
2、 Influence of material characteristics
physical properties
Hardness: The higher the hardness of the material (such as quartz), the faster the wear of the hammer head.
Particle size: The feed particles are too large or contain impurities (such as iron blocks), which increases the impact load.
Moisture content: Wet materials are prone to adhesion, exacerbating friction between the hammer head and the lining plate.
chemical composition
The material with high silica content in grade 2 has strong corrosiveness to the hammer head.
3、 Equipment operating parameters
Improper rotor linear velocity
High speed: The material cannot enter the impact zone, and the wear on the top of the hammer head intensifies.
Low rotation speed: The material penetrates deep into the base of the hammer head, causing severe wear on the side.
Gap adjustment failure
The gap between the hammer head and the grate or lining plate is too small: the material is blocked, and the hammer head is repeatedly rubbed.
Excessive gap: Low crushing efficiency, increased ineffective impact of hammer head.
Mismatch in processing capability
Overloaded operation or uneven feeding can cause local overheating and phase change wear of the hammer head.
4、 Operational and maintenance omissions
installation error
Inconsistent or poorly secured hammer angles can lead to unbalanced stress and accelerate the risk of fracture.
Maintain deficiencies
Failure to regularly check for loose bolts and insufficient lubrication exacerbates vibration wear.
Failure to replace or repair in a timely manner after wear and tear can lead to chain damage.
Key preventive measures
Preferred Material: Double metal composite hammer head (high chromium head+alloy steel handle) or customized material (such as hard material with high toughness alloy).
Control parameters: Adjust the rotor speed to a reasonable range (refer to the equipment manual) and maintain a discharge gap of 5-10mm.
Material pretreatment: Screen out impurities, control feed particle size ≤ design value, moisture content < 10%.
Standardized operation: Uniform feeding, regular tightening of bolts, and inspection of lubrication system.